Characteristics
|
Chemical composition |
|
Polyester-polyurethane in aqueous dispersion |
|
pH at 20°С |
|
6,0 - 9,0 |
|
RVT Brookfield viscosity at 20°С, 20 rpm |
mPa.s |
1200 – 2000 |
|
Specific gravity |
g/cm3 |
1,05 – 1,07 |
|
Solid content |
% |
40±1 |
|
MFT |
°С |
4 - 5 |
|
Reactivation temperature |
°С |
60 – 80 |
|
Stability at 20°С |
months |
6 |
Use
|
application |
|
spray coating |
|
Temperature of materials, room and glue |
°С |
18 - 22 |
|
Wood moisture |
% |
8 - 12 |
|
Quantity of sprayed adhesive |
g/m2 |
80 - 120 |
|
Reactivation temperature |
°С |
60 – 80 |
|
Pressure (1) |
Бар |
7-15 |
|
Pressing time (2) |
sec. |
60 - 120 |