Characteristics
Chemical composition |
|
Polyester-polyurethane in aqueous dispersion |
pH at 20°С |
|
6,0 - 9,0 |
RVT Brookfield viscosity at 20°С, 20 rpm |
mPa.s |
900 - 1300 |
Specific gravity |
g/cm3 |
1,05 – 1,07 |
Dry polymer |
% |
40±1 |
MFT |
°С |
4 - 5 |
Reactivation temperature |
°С |
60 – 80 |
Stability at 20°С |
months |
6 |
Mixture life |
hours |
около 24 |
Reactivation time after application |
hours |
? 36 |
application |
|
распыление |
Temperature of materials, room and glue |
°С |
18-22 |
Wood moisture |
% |
8-12 |
Quantity of sprayed adhesive |
g/m2 |
80 - 120 |
Reactivation temperature |
°С |
60 – 80 |
Pressure |
Bar |
4 |
Pressing time |
sec |
60 - 120 |
The conditions for optimum use of DUDIPUR D 12/4 are:
Dudipur D 12/4 |
100 |
p. by weight |
Vildur L 202 |
3-5 |
p. by weight |