Characteristics
|
Chemical composition |
|
Polyester-polyurethane in aqueous dispersion |
|
рН at 20 °С |
|
6,0 - 8,0 |
|
RVT Brookfield viscosity at 20°С, 20rpm |
mPa.s |
~ 1400 |
|
Solid content |
% |
40±1 |
|
MFT |
°С |
4 - 5 |
|
Reactivation temperature |
°С |
60 – 80 |
|
Stability at 20 °С |
|
6 months |
Use
|
Application |
|
Spray coating |
|
Temperature of materials, room and glue |
°С |
18-22 |
|
Wood moisture |
% |
8-12 |
|
Quantity of sprayed adhesive |
g/m2 |
40 - 120 |
|
Reactivation temperature |
°С |
60 – 80 |
|
Pressure (1) |
кг/см2 |
7 - 15 |
|
Pressing time (2) |
минут |
1 - 2 |
(1) Depending on the type of press used
(2) As a function of temperature, pressure and PVC thickness